Superalloys resist wear at nearly forge-level heat using new process
https://phys.org/news/2025-01-superalloys-resist-forge.html
"spinel oxides self-lubricate under heat stress/ friction when paired with Inconel 718 nickel-chromium-based superalloys... maintains lubrication up to 700°C without corrosion... aerospace, nuclear energy"